Atomic Layer Deposition and Properties of Lanthanum Oxide and Lanthanum-Aluminum Oxide Films
2006
Atomic layer deposition (ALD) of lanthanum oxide on glass and silicon substrates was examined using lanthanum silylamide, La[N(SiMe 3 ) 2 ] 3 , and water as precursors in the substrate temperature range of 150-250 °C. The effect of pulse times and precursor evaporation temperature on the growth rate and refractive index was investigated. The films remained amorphous regardless of the deposition conditions. The resulting La 2 O 3 films contained noticeable amounts of hydrogen and silicon and were chemically unstable while stored in ambient air. Lanthanum aluminum oxide films were achieved with stoichiometry close to that of LaAlO 3 at 225°C from La[N(SiMe 3 ) 2 ] 3 , Al(CH 3 ) 3 , and H 2 O.…
Structural, optical, and luminescence properties of ZnO:Ga optical scintillation ceramic
2018
This paper discusses the characteristics of ZnO and ZnO:Ga ceramics fabricated by uniaxial hot pressing. The short-wavelength transmission limit of zinc oxide ceramics is in the 370-nm region; the long-wavelength limit is determined by the free-charge-carrier concentration and lies in the interval from 5 to 9 μm. The total transmittance of such ceramics in the visible and near-IR regions is about 70% when the sample is 0.5 mm thick. The luminescence spectrum is represented by a broad emission band with maximum at 580 nm, having a defect nature. The introduction of 0.03–0.1 mass % gallium into the zinc oxide structure inhibits grain growth and increases the free-charge-carrier concentration …
MOCVD growth of CdO very thin films: Problems and ways of solution
2016
Abstract In this paper the growth of CdO by the MOCVD technique at atmospheric pressure has been studied in order to achieve very thin films of this material on r-sapphire substrates. The growth evolution of these films was discussed and the existence of a threshold thickness, below which island-shaped structures appear, was demonstrated. Some alternatives to reduce this threshold thickness have been proposed in the frame of the analysis of the crystal growth process. The morphology and structural properties of the films were analyzed by means of SEM and HRXRD. High-quality flat CdO samples were achieved with thicknesses up to 20 nm, which is five times thinner than the values previously re…
Characteristics of industrially manufactured amorphous hydrogenated carbon (a-C:H) depositions on high-density polyethylene
2016
Industrially high-density polyethylene (HDPE) was successively covered by two types of amorphous hydrogenated carbon (a-C:H) films, one more flexible (f-type) and the other more robust (r-type). The films have been grown by radio frequency plasma-enhanced chemical vapor deposition (RF-PECVD) technique with acetylene plasma. The surface morphology of both types has been studied by atomic force microscopy (AFM) and scanning electron microscopy (SEM). Contact angle measurements and Raman spectroscopy analysis were done to investigate the surface wettability and carbon chemical composition. Both types display similar morphology and grain growth pattern. Contact angle measurements revealed surfa…
Acoustic vibrations of monoclinic zirconia nanocrystals
2011
International audience; Polarized low-frequency Raman spectra originating from confined acoustic vibrations are reported for monoclinic ZrO2 nanoparticles with a narrow size distribution synthesized from a continuous supercritical water process. The monoclinic lattice structure is taken into account for the interpretation of the spectra by comparing with isotropic and anisotropic continuum elasticity calculations for monodomain nanocrystals. The various mechanisms leading to the broadening of the Raman peaks are discussed. We demonstrate that an accurate determination of the size distribution of the nanoparticles is possible using the Raman peak due to the fundamental breathing vibration wh…
Isothermal relaxation of discommensurations in K2ZnCl4
1994
At the incommensurate-ferroelectric transition temperature T c of K 2 ZnCl 4 , the dielectric susceptibility contains an anomalous contribution both above and below T c . Previous quasi-static dielectric measurements and hysteresis loops demonstrated that this anomalous part arises from the peculiar dynamics of discommensurations. We have used isothermal dielectric measurements to get some insight into the long time dynamics of these discommensurations. We have found that the characteristic relaxation times τ are of the order of 10 4 s in the incommensurate and in the ferroelectric phase. Even more unusual is a non-monotonous relaxation which is observed in a restricted temperature range ab…
Structural characterization of TiO2/TiN O (δ-doping) heterostructures on (1 1 0)TiO2 substrates
2003
Abstract TiO2/TiNxOy δ-doping structures were grown on the top of (1 1 0)TiO2 rutile substrates by low pressure metal-organic vapor phase epitaxy (LP-MOVPE) technique at 750 °C. The samples were analyzed by high resolution transmission electron microscopy (HRTEM), electron energy loss spectroscopy (EELS) and X-ray diffraction techniques (rocking curves and φ-scans). The presence of satellites in the (1 1 0)TiO2 rocking curve revealed the epitaxial growth of 10 period δ-doping structures. The thickness of the TiO2 layers, 84 nm, was deduced from the satellites period. HRTEM observations showed around 1.5 nm thick δ-doping layers, where the presence of nitrogen was detected by EELS. The analy…
How activator ion concentration affects spectroscopic properties on Ba4Y3F17: Er3+, Yb3+, a new perspective up-conversion material
2018
Abstract Ba4Y3F17 with Er3+ and Yb3+, a promising material for up-conversion luminescence, was synthesized. Excellent isomorphic capacity was detected. Low-temperature measurements show that erbium ions are incorporated in multiple lattice positions, which is inconsistent with the current model of Ba4Y3F17 crystal lattice structure. Activator ion concentration has a different impact on 4S3/2 and 4F9/2, states (for the green and red luminescence, respectively) depopulation. Energy transfer from Er3+ 4S3/2 state to Yb3+ is observed even at low temperature (15 K) while Er-Er cross-relaxation is observed from 120 K and above. Yb3+ concentration has a great impact to red-to-green up-conversion l…
Influence of spray trajectories on characteristics of cold-sprayed copper deposits
2021
Abstract Industrial robots are widely used in cold spray (CS) as well as thermal spray to produce various coatings by precisely controlling kinematic parameters during the process. However, the robot trajectory and its effect on the characteristics of CS deposits are important, but not fully studied. This article introduces four typical spray trajectories, including zigzag path, cross path, parallel path, and spiral path, to elaborate thick CS Cu deposits, and characterizes the corresponding Cu deposits, respectively. The experimental results revealed that the spray trajectories have a major influence on the associated thermal history and the residual stress distribution. However, no signif…
High temperature oxidation of Mg2(Si-Sn)
2016
Abstract High temperature oxidation of Mg 2 Si 1- x Sn x alloys ( x = 0.1 0.6) has been investigated. The oxidation rate was slow for temperatures below 430 °C. In the temperature range between 430500 °C all the alloys exhibited breakaway oxidation. The onset temperature of the breakaway region in general decreased with increasing level of Sn in the alloy. The breakaway behavior is explained by a combination of the formation of a non-protective MgO layer and the formation of Sn-rich liquid at the interface between the oxide and Mg depleted Mg 2 Sn.